Ultrathin oxide films by atomic layer deposition on graphene

Luda Wang, Jonathan J. Travis, Andrew S. Cavanagh, Xinghui Liu, Steven P. Koenig, Pinshane Y. Huang, Steven M. George, J. Scott Bunch