Skip to main navigation Skip to search Skip to main content

Nanoindentation and Nano-Compresion Testing of Ni3Al Precipitates

  • B. Gan
  • , H. Murakami
  • , R. Maaß
  • , L. Meza
  • , J. R. Greer
  • , T. Ohmura
  • , S. Tin

Research output: Chapter in Book/Report/Conference proceeding › Chapter

Abstract

Using an AFM-based instrumented nanoindentation system, the nanoindentation response of γ' particles (Ni3Al) in a Ni-base single crystal superalloy CMSX-4 was characterized to demonstrate the influence of the softer γ matrix on the measurement of nano-mechanical properties of γ' particles. The properties of the γ' particles were measured after both a standard and a coarsening heat treatment, in which the initially sub-micron sized cuboidal γ' particles transformed to large, irregularly shaped γ' precipitates with dimensions in excess of 30 μm. The measured nano-hardness of the coarsened γ' precipitates in CMSX-4 appears to increase slightly with the increasing load. Nano-compression testing of cuboidal γ' particles, electrolytically extracted from a CMSX-4 after a standard solution and age heat treatment, was also performed. With a maximum value of 10 GPa, the measured yield stress of these dislocation-free γ' particles approaches the ideal strength and is equivalent to -G/17. Compared to the measured yield strengths of γ' phase in its bulk crystal form, these nano-compression results are more than a factor of 33 higher. Additionally, the 'softening' effect of Ga+ ion implantation on the strength of dislocation-free nanocrystals was also assessed. The resulting yield strengths of cuboidal γ' precipitates imaged with a focused ion beam were at least 5 GPa lower than those that had not been subjected to Ga+ ion implantation.

Original languageEnglish (US)
Title of host publicationSuperalloys 2012
PublisherJohn Wiley & Sons, Ltd.
Pages83-91
Number of pages9
ISBN (Print)9780470943205
DOIs
StatePublished - Oct 2 2012
Externally publishedYes

Keywords

  • Nano-compression
  • Nanoindentation
  • Superalloy
  • γ′ precipitate

ASJC Scopus subject areas

  • General Materials Science

Fingerprint

Dive into the research topics of 'Nanoindentation and Nano-Compresion Testing of Ni3Al Precipitates'. Together they form a unique fingerprint.

Cite this