@article{d68a6bc9fd9b4168a7c7b4348532f537,
title = "Mechanism of plastic deformation of a Ni-based superalloy for VHTR applications",
author = "Kun Mo and Xiang Chen and Gianfranco Lovicu and Tung, {Hsiao Ming} and Stubbins, {James F.}",
note = "The work was supported by the US Department of Energy under Grants DE-FC07-07ID14819 and DOE NEUP 09-516 . The authors would like to thank Dr. Peter Kurath from the Advanced Materials Testing and Evaluation Laboratory of University of Illinois at Urbana-Champaign for technical assistance. The authors would also like to thank Haynes International, Inc. for providing testing materials. The microstructural analysis was carried out in part in the Frederick Seitz Materials Research Laboratory Central Facilities, University of Illinois, which are partially supported by the U.S. Department of Energy under Grants DE-FG02-07ER46453 and DE-FG02-07ER46471 .; 2010 ANS Annual Meeting and Embedded Topical Meetings ; Conference date: 13-06-2010 Through 17-06-2010",
year = "2010",
language = "English (US)",
volume = "102",
pages = "850--851",
journal = "Transactions of the American Nuclear Society",
issn = "0003-018X",
publisher = "American Nuclear Society",
}